    来源:https://www.fumeijia.net/ 日期:2021-12-20 发布人:admin
    一、板材含水率。
    1、 Moisture content of plate.
    家具板的含水率决定了板的胶合强度等方面。一旦板材含水率不达标或超标,就会造成板材质量问题,不仅是实木生态板、多层板,其他板材也是如此。
    The moisture content of furniture board determines the bonding strength of the board. Once the moisture content of the board does not meet the standard or exceeds the standard, it will cause the quality problem of the board, not only the solid wood ecological board and multilayer board, but also other boards.
    一般来说,多层板的含水率标准为8%-12%,不同地区的气候和空气湿度不同,因此不同地区板含水率的具体操作方法也不完全相同。更好的办法是晾晒,与空气充分接触,然后进行其他操作,这与以下几点密切相关。
    Generally speaking, the moisture content standard of multilayer board is 8% - 12%. The climate and air humidity in different regions are different, so the specific operation methods of moisture content of multilayer board in different regions are not exactly the same. The better way is to dry, fully contact with the air, and then carry out other operations, which is closely related to the following points.
    二、板材生产工艺-干燥。
    2、 Plate production process - drying.
    在多层板或生态板的生产过程中,一个基本涉及的过程就是干燥,不仅用于板材的原材料,还用于板材的半成品。
    In the production process of multilayer board or ecological board, a basic process involved is drying, which is not only used for raw materials of board, but also used for semi-finished products of board.
    富美家快装板
    举例来说,就多层板而言,是一层层单板涂胶后,再贴上中板,再贴上面皮。在中板和底板之间,需要进行的一个过程是干燥,因为单板和单板之间干燥、涂胶成的底板一般都是存放在空气中,与空气充分接触,自然调节含水率。然后干燥,粘贴中板和面皮,这样多层板的质量可以得到保证。
    For example, for multi-layer boards, glue the veneer layer by layer, then paste the middle board, and then paste the dough. Drying is a necessary process between the middle plate and the bottom plate, because the dried and glued bottom plate between the veneer and the veneer is generally stored in the air and fully contacted with the air to naturally adjust the moisture content. Then dry and paste the middle board and the dough, so that the quality of the multi-layer board can be guaranteed.
    但目前有些厂家由于工期较紧,所以底板生产后直接粘贴中板进行贴面,导致胶合强度不足,容易开胶。
    However, due to the tight construction period, some manufacturers directly paste the middle plate for veneering after the production of the bottom plate, resulting in insufficient bonding strength and easy to open the glue.
    三、胶粘剂选择不当。
    3、 Improper choice of adhesive.
    无论是多层板还是生态板,一旦胶粘剂选择不当,很容易造成板材开胶。
    Whether it is multilayer board or ecological board, once the adhesive is improperly selected, it is easy to cause the board to open.
    四、外部环境对板材的影响。
    4、 Influence of external environment on plate.
    很多时候,我们觉得买了家具板之后,其他地区的朋友用的很好,自己做不到。这和外界环境有很大关系。
    Many times, we feel that after buying furniture boards, our friends in other areas use them very well, and we can't do it ourselves. This has a lot to do with the external environment.
    众所周知,板材的含水率约为8%-12%,但外界空气的含水率却不那么固定,我国地域辽阔,大江南北的气候、温差、空气湿度等方面都有很大的差异,因此在个别地区也会对板材产生影响,这与板材本身的质量无关。
    As we all know, the moisture content of the plate is about 8% - 12%, but the moisture content of the outside air is not so fixed. China has a vast territory, and there are great differences in climate, temperature difference and air humidity between the north and the south of the river. Therefore, it will also affect the plate in some areas, which has nothing to do with the quality of the plate itself.
    我们一直在坚持分享的路上富美家快装板http://www.fumeijia.net真正为您解决您所需要的问题.
    We have been insisting on the way of sharing. Fumeijia fast loading board http://www.fumeijia.net Truly solve the problems you need
    联系我们

    产品销售热线:18660816658

    技术方案咨询:18560211715

    仓库地址:济南市槐荫区河海工业园9号

    九江工厂:九江市江东大道3号

    台湾新竹工厂:台湾新竹

    泰国曼谷工厂:泰国曼谷

    关注我们
    山东创图建筑装饰工程有限公司 备案号:鲁ICP备14019259号-2 网站地图 XML TXT 鲁公网安备37010502002020号

    截屏,微信识别二维码

    微信号:18660816658